Item | Fire Clay Brick SK-32 | Fire Clay Brick SK-34 | Fire Clay Brick SK-36 |
AI2O3(%) | 30 | 38 | 50 |
Fe2O3 (%) | 3 | 2.5 | 2 |
Refractoriness (SK) | 32 | 34 | 36 |
Refractoriness under load, 0.2MPa, Ta, ((°C) | 1300 | 1350 | 1450 |
Porosity (%) | 22-26 | 19-23 | 20-24 |
Bulk density (g/cm³) | 2.05 | 2.10-2.15 | 2.30-2.40 |
Cold crushing strength (MPa) | 25 | 25 | 45 |
Thermal expansion at 1000°C (%) | 0.6 | 0.6 | 0.3 |